asme ix (interpretação vol.55)

3
7/28/2019 ASME IX (Interpretação Vol.55) http://slidepdf.com/reader/full/asme-ix-interpretacao-vol55 1/3 SECTION IX Subject Interpretation File No. QW-100.3 and QW-200.2, Procedure Qualification Record Time Limits . . . . . . . . . . . . . . . . . . . IX-04-10 BC04-601 QW-200.4, Combination of Welding Procedures . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . IX-04-08 BC03-1770 QW-403.6, QW-451, and QW-401.3; Notch Toughness Testing . . . . . . . . . . . . . . . . . . . . . . . . . . IX-04-04 BC03-1246 QW-403.9, Base Metal Thickness . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . IX-04-09 BC04-065

Upload: lsinsp3381

Post on 03-Apr-2018

221 views

Category:

Documents


0 download

TRANSCRIPT

Page 1: ASME IX (Interpretação Vol.55)

7/28/2019 ASME IX (Interpretação Vol.55)

http://slidepdf.com/reader/full/asme-ix-interpretacao-vol55 1/3

SECTION IX

Subject Interpretation File No.

QW-100.3 and QW-200.2, Procedure Qualification Record Time Limits . . . . . . . . . . . . . . . . . . . IX-04-10 BC04-601

QW-200.4, Combination of Welding Procedures . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . IX-04-08 BC03-1770

QW-403.6, QW-451, and QW-401.3; Notch Toughness Testing . . . . . . . . . . . . . . . . . . . . . . . . . . IX-04-04 BC03-1246

QW-403.9, Base Metal Thickness . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . IX-04-09 BC04-065

Page 2: ASME IX (Interpretação Vol.55)

7/28/2019 ASME IX (Interpretação Vol.55)

http://slidepdf.com/reader/full/asme-ix-interpretacao-vol55 2/3

Interpretation: IX-04-04

Subject: QW-403.6, QW-451, and QW-401.3; Notch Toughness Testing

Date Issued: September 15, 2003File: BC03-1246

Backgraound: A WPS is supported by three PQRs. Two PQRs are recorded on 12-mm and 28.5-mm

thick coupons using tensile, bend, and impact testing specimens. A third PQR was made using 5-mm thick 

plate using the same welding parameters, but only impact specimens were tested.

Question (1): May these PQRs be combined to support a WPS for welding 2.5 mm through 57 mm

material requiring notch toughness testing?

Reply (1): No.

Question (2): May these three PQRs be combined to support welding base metal thicknesses of 4.8 mm

through 57 mm with or without notch toughness?

Reply (2): Yes.

Note: This interpretation originally appeared in Volume 54. The “WP” in Question (1) has been corrected

by Errata to read “WPS.”

Interpretation: IX-04-08

Subject: QW-200.4, Combination of Welding Procedures

Date Issued: April 1, 2004

File: BC03-1770

Question: A combination weld process PQR was qualified using the GTAW for the root pass, SMAW,

and SAW. May this PQR support a WPS for welding with only one or two of the processes shown on the PQR?

Reply: Yes, provided the following are met:

(a) The remaining essential, nonessential, and supplementary essential variables, when applicable, are

applied.

(b) The base metal and deposited weld metal thickness limits of QW-451 are applied.

Page 3: ASME IX (Interpretação Vol.55)

7/28/2019 ASME IX (Interpretação Vol.55)

http://slidepdf.com/reader/full/asme-ix-interpretacao-vol55 3/3

Interpretation: IX-04-09

Subject: QW-403.9, Base Metal Thickness

Date Issued: April 1, 2004

File: BC04-065

Question: An EGW procedure was qualified on 3 ⁄ 8-in. thick base material completing the weld joint in

one single pass. Is the WPS qualified to make a weld deposit greater than 1 ⁄ 2 in., in one pass, in base metal

greater than 1 ⁄ 2 in. in thickness?

Reply: No.

Interpretation: IX-04-10

Subject: QW-100.3 and QW-200.2, Procedure Qualification Record Time Limits

Date Issued: June 10, 2004

File: BC04-601

Question: Is there a time limit on the validity of a PQR?

Reply: PQRs always remain valid but may only be used to support WPSs, provided they meet the

requirements of the 1962 or later Edition of ASME Boiler and Pressure Vessel Code Section IX. See QW-

100.3.